The limitations of die-casting described in the text are primarily related to shrinkage dependent on the geometry of the piece and the brittleness of certain metal alloys, with draft angles being largely unnecessary except for very deep sections.
Regarding shrinkage, the text states that "the amount of shrinkage is often dependent upon the shape of the piece" . Pieces with central cores, such as those illustrated in Figures 20 and 24, "will shrink very little," whereas pieces without internal supports "will shrink to the greatest extent" . Consequently, specific geometric features must be accounted for during design . In terms of die release, "Practically no draft is necessary on a die-casting, except on very deep sections," where a draft of 0.001 inch to the inch is desirable .
In terms of material limits, alloys containing "15 to 40 per cent copper and 60 to 85 per cent zinc are brittle, having low strength and low ductility" . While aluminum is castable, it is noted as "a difficult metal to run into thin walls and fine details" . These are the specific limitations provided in the passages; the text does not list other operational limits such as machine size or temperature ceilings in the provided excerpts.