The standard method is to dissolve 1/4 lb. of alum and 1 oz. cream of tartar for every pound of wool in water; enter the wool when the water is warm, raise to boiling and boil for one hour, then take the bath off the fire and allow it to cool overnight . After cooling, wring out the wool (do not wash it) and store it in a linen bag in a cool place for 4 or 5 days, after which wash it thoroughly before dyeing . The cream of tartar is added because it "helps to brighten the ultimate colour" . Specific recipes vary slightly: for example, madder red uses 1/4 lb. alum per pound of wool boiled for 1 hour, cooled in the mordant, then bagged for 3 or 4 days ; and the logwood purple recipe uses 1/4 lb. alum and 1/2 oz. tartar for one hour . The passages do not cover all possible alum mordanting variations.

有帮助 0引用
Vegetable Dyes Assistant官方匹配 0.76

The passages provided do not include a single, general instruction for mordanting wool with alum. Instead, they specify alum quantities, times, and sometimes additional agents for particular colors and fabric weights in various recipes; no universal method is stated.

The specific alum-mordanting instructions mentioned are:

  • For "Yellow for Wool" (heather): "mordant with 5 oz. alum for 1 hour and wash" .
  • For "Yellow for Wool" (weld): "Boil wool with 4% of alum for 1 to 2 hours" .
  • For "Yellow for Wool" (weld): "Mordant with alum and tartar" .
  • For "Fustic Green for Wool": "Mordant wool with 11 lbs. alum" for 50 lbs. of wool .
  • For "Saxon Green for Wool": "Mordant the wool with alum and tartar for half-an-hour; it is then taken out and aired, but not washed" .
  • For "Green with Quercitron for Wool": "For 100 parts of wool, put 3 parts of chalk and 10 or 12 of alum. Boil the wool in this for 1 hour" .
  • For "Red with Madder for Wool": "Mordant the wool with Alum, adding some cayenne pepper" .
  • For "Pink with Cochineal for Wool": "5 lbs. 12 oz. alum. Boil and immerse wool for 50 minutes" .
  • For "Ordinary Logwood Purple for Wool": "Mordant wool with ¼ lb. alum and ½ oz. tartar for 1 hour; wring out and put away in a bag for some days" .
  • For "Logwood Purple for Wool" (alternative mordants listed): "With alum mordant (4 oz.) a crimson colour is got" .
  • For "Catechu Stone Drab" (cotton, not wool): "Add ½ oz. alum" after other steps .
  • For "Green for Linen with Larch Bark" (linen, not wool): "Mordant 4 lbs. linen with ½ lb. alum. Boil for 2½ hours" .
  • For "Yellow for Cotton" (cotton, not wool): "It is alumed with ¼ of its weight of alum. After 24 hours it is taken out of the bath and dried without washing" .
  • For "Red for Silk" (silk, not wool): "mordanted over night with alum, by steeping it in a cold concentrated solution; wash well" .
  • For "Old Gold for Wool" (chrome, not alum): "Mordant with 2% chrome" .
  • For "Golden Yellow for Wool" (bichromate, not alum): "mordant with 3 oz. bichromate of potash" .
  • For "Purple, for Wool" (cochineal, various mordants): "With alum mordant (4 oz.) a crimson colour is got" .
  • For "Scarlet, for Wool" (stannous chloride, not alum): "Mordant the wool for 1 to 1½ hours with 6% stannous chloride and 4% cream of tartar" .

These practices are from A Book on Vegetable Dyes by Ethel M. Mairet, reflecting dyer's techniques as they were when the book was written; modern safety and environmental practices for mordants like alum may have changed.

有帮助 0引用
Textiles Assistant官方匹配 0.58

The provided passages do not give a specific procedure for mordanting wool with alum; they only state that alum can serve as a mordant and define what a mordant does.

Footnote [25] explains that "Alum in this case is called a mordant, which is a substance that will impregnate the cloth with something which will hold the coloring matter" . It also lists that "Other mordants are oxides, hydroxides, and basic salts of aluminum, iron, tin, and chromium" . The "Dyeing and Finishing" section notes that "Few of the natural dyestuffs attach themselves permanently without use of a mordant" and defines a mordant as "a substance which has an affinity for, or which can penetrate, the fiber to be colored, and which possesses the power of combining with the dyestuff and thus forming an insoluble compound upon the fiber" . While Experiment 21 describes mordanting cotton cloth with common alum, it does not provide a corresponding method for wool .